(Created page with " Max temp/Time 1000C = 1 Hour 1100C = 10 min 1200C = 3 min 1300C = 10 seconds")
(No difference)

Revision as of 14:17, 28 June 2012


Max temp/Time

1000C = 1 Hour 1100C = 10 min 1200C = 3 min 1300C = 10 seconds