RIE 2 (MRC)
CdZnTe Etching (RIE 2)
ZnS Etching (RIE 2)
ITO Etching (RIE 2)
InP-InGaAsP-InGaAlAs Etching (RIE 2)
RIE 3 (MRC)
SiO2 Etching (RIE 3)
SiNx Etching (RIE 3)
RIE 5 (PlasmaTherm)
AlGaAs\GaAs Etching (RIE 5)
GaN Etching (RIE 5)
Photoresist and ARC (RIE 5)
DUV42P (AR2) etching
- O2 = 20sccm // Pressure = 10mT // RF = 100W // Time = 40 sec
- No need to pump/purge, can etch right away.
- No helium cooling, Run in manual mode.