==CdZnTe Etching (RIE 2)== |
==CdZnTe Etching (RIE 2)== |
||
*[[media:11-CZT_etching-1.pdf|CdZnTe Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
*[[media:11-CZT_etching-1.pdf|CdZnTe Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
||
+ | |||
+ | ==InP-InGaAsP-InGaAlAs Etching (RIE 2)== |
||
+ | *[[media:RIE2-InGaAs-InP-InAlAs-Etch-Plasma-RIE-RevA.pdf|InP-InGaAsP-InAlGaAs Etch Recipes - CH<sub>4</sub>-H<sub>2</sub>-Ar]] |
||