Difference between revisions of "Photoluminescence PL Setup (Custom)"
Jump to navigation
Jump to search
(→Pump Lasers Available: added 532nm laser) |
|||
(2 intermediate revisions by the same user not shown) | |||
Line 2: | Line 2: | ||
|picture=Holograph.jpg |
|picture=Holograph.jpg |
||
|type = Inspection, Test and Characterization |
|type = Inspection, Test and Characterization |
||
− | |super= |
+ | |super= Demis D. John |
− | |phone=(805) 839-5689 |
||
|location=Bay 6 |
|location=Bay 6 |
||
+ | |description = Free-space optical Photoluminescence |
||
− | |email=Ningcao@ece.ucsb.edu |
||
− | | |
+ | |manufacturer = Custom-Built Optics |
}} |
}} |
||
==About== |
==About== |
Latest revision as of 20:45, 26 September 2023
|
About
The Photoluminescence setup is on the same optical table as the Hologaphic Lithography setup.
This custom setup is used for materials characterization including crystal growth quality and gain region/quantum well growth, or semiconductor alloy ratio. Multiple laser sources are available - including the He-Cd laser also used for Holography, via a flip-down mirror.
Light is delivered in free-space, selected via magnetic flip-mirrors, and collected by optical fiber, and analyzed by a USB spectrometer.
Detailed Specifications
Pump Lasers Available
- 325nm He-Cd - single mode, spatially filtered
- 405nm Diode Laser
- 532nm Diode Laser
- 657nm Diode Laser
Optical Detection
- Ocean Optics USB2000+
- 340nm to 1025nm wavelength acquisition, through multi mode optical fiber
- Raman spectrometer