The oven temperature can be controlled from 30C-200C with a user programable ramp rate between 0.1C-1.0C/min. Maximum temperature is 200C. There is a N2 purge to provide a dry intert atmosphere during use.
 +
 
=Documentation=
 
=Documentation=
*[[ media: Watlow_982_controller.pdf|Operating Instructions]]
+
*[[ media: Watlow_982_controller.pdf|Operating Instructions: Chapter 7 is specific to Nanofab users]]
 +
*[[ media: Oven5.pdf|Oven 5 Manual]]
 +
 
 +
=Oven 5=
 +
{{tool|{{PAGENAME}}
 +
|picture=Oven5.jpg
 +
|type = Lithography
 +
|super= Brian Lingg
 +
|location=Bay 5
 +
|description = ?
 +
|manufacturer =Labline
 +
}}

Latest revision as of 08:20, 17 March 2017

About

The oven temperature can be controlled from 30C-200C with a user programable ramp rate between 0.1C-1.0C/min. Maximum temperature is 200C. There is a N2 purge to provide a dry intert atmosphere during use.

Documentation

Oven 5

Oven 5 (Labline)
Oven5.jpg
Tool Type Lithography
Location Bay 5
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description ?
Manufacturer Labline