+ | =About= |
− | This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and |
+ | This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 100°C-350°C operation. This chamber has 100% SiD<sub>4,</sub> N<sub>2</sub>, O<sub>2</sub>, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO<sub>2</sub> and Si<sub>3</sub>N<sub>4</sub>, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 100°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized. |
+ | ===Cluster Configuration=== |
||
⚫ | |||
+ | A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey. |
||
+ | *'''PM3''': ICP-PECVD Deposition (this page) |
||
⚫ | |||
+ | *'''PM1''': [[ICP-Etch (Unaxis VLR)|ICP Etch (Unaxis VLR)]] |
||
⚫ | |||
+ | |||
⚫ | |||
⚫ | |||
+ | |||
⚫ | |||
⚫ | |||
⚫ | |||
*Multiple 4” diameter wafer capable system |
*Multiple 4” diameter wafer capable system |
||
*Pieces possible by mounting or placing on 4 ” wafer |
*Pieces possible by mounting or placing on 4 ” wafer |
||
=Documentation= |
=Documentation= |
||
+ | |||
− | *[[media:UnaxisVLRInstructions.pdf|Operating Instructions]] |
||
+ | *[[Unaxis VLR ICP-PECVD - Std. Operating Procedure|Operating Instructions]] |
||
+ | *[[Unaxis wafer coating procedure]] - ''process flow for achieving high-quality coatings.'' |
||
+ | **For particle counting procedure, see the [https://wiki.nanotech.ucsb.edu/wiki/Wafer_scanning_process_traveler Surfscan Scanning Procedure] |
||
+ | |||
+ | == Recipes == |
||
+ | You can find recipes for this tool on the Wiki > Recipes > [https://wiki.nanotech.ucsb.edu/wiki/PECVD_Recipes#ICP-PECVD_.28Unaxis_VLR.29 PECVD Recipes page] |
Revision as of 00:08, 16 July 2020
|
About
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 100°C-350°C operation. This chamber has 100% SiD4, N2, O2, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO2 and Si3N4, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 100°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized.
Cluster Configuration
A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey.
- PM3: ICP-PECVD Deposition (this page)
- PM1: ICP Etch (Unaxis VLR)
Detailed Specifications
- 1000W ICP source, 600W RF Sample Bias Power Supply
- 100 - 350°C sample temperature
- 100% SiD4, Ar, N2, O2
- Multiple 4” diameter wafer capable system
- Pieces possible by mounting or placing on 4 ” wafer
Documentation
- Operating Instructions
- Unaxis wafer coating procedure - process flow for achieving high-quality coatings.
- For particle counting procedure, see the Surfscan Scanning Procedure
Recipes
You can find recipes for this tool on the Wiki > Recipes > PECVD Recipes page