[[File:Au oxidation by O2-N2 ash.jpg|left|thumb|1177.81x1177.81px|In high oxidation environment, gold surface can darken or oxidized, as shown by the XPS data. Recipes with O2_N2 gas mixture often produce this effect.]]
+
[[File:Au oxidation by O2-N2 ash.jpg|left|thumb|900x900px|In high oxidation environment, gold surface can darken or oxidized, as shown by the XPS data. Recipes with O2_N2 gas mixture often produce this effect.|alt=|border]]

Latest revision as of 16:22, 9 June 2023

In high oxidation environment, gold surface can darken or oxidized, as shown by the XPS data. Recipes with O2_N2 gas mixture often produce this effect.