Difference between revisions of "Gold surface oxidation (darkening) due to O2/N2 plasma; the need for O2 only recipe."
Jump to navigation
Jump to search
(Gold surface darkened after O2/N2 ashing recipe treatment, XPS data showed that Au can oxidize in the high oxidization condition) |
|||
(One intermediate revision by the same user not shown) | |||
Line 1: | Line 1: | ||
+ | [[File:Au oxidation by O2-N2 ash.jpg|left|thumb|900x900px|In high oxidation environment, gold surface can darken or oxidized, as shown by the XPS data. Recipes with O2_N2 gas mixture often produce this effect.|alt=|border]] |