(Gold surface darkened after O2/N2 ashing recipe treatment, XPS data showed that Au can oxidize in the high oxidization condition) |
(scale) |
||
Line 1: | Line 1: | ||
+ | [[File:Au oxidation by O2-N2 ash.jpg|left|thumb|1177.81x1177.81px|In high oxidation environment, gold surface can darken or oxidized, as shown by the XPS data. Recipes with O2_N2 gas mixture often produce this effect.]] |