Difference between revisions of "Film Stress (Tencor Flexus)"
Jump to navigation
Jump to search
(Created page with "{{tool|{{PAGENAME}} |picture=Tencor.jpg |type = Inspection, Test and Characterization |super=Mike Silva |phone=(805)839-3918x219 |location=Bay ? |email=silva@ece.ucsb.edu |descri…") |
(moved to bay 1) |
||
(5 intermediate revisions by 4 users not shown) | |||
Line 2: | Line 2: | ||
|picture=Tencor.jpg |
|picture=Tencor.jpg |
||
|type = Inspection, Test and Characterization |
|type = Inspection, Test and Characterization |
||
− | |super= |
+ | |super= Lee Sawyer |
|phone=(805)839-3918x219 |
|phone=(805)839-3918x219 |
||
− | |location=Bay |
+ | |location=Bay 1 |
|email=silva@ece.ucsb.edu |
|email=silva@ece.ucsb.edu |
||
|description = Film Stress Measurement system |
|description = Film Stress Measurement system |
||
|manufacturer = Tencor |
|manufacturer = Tencor |
||
+ | |model = FLX-2320 |
||
|materials = |
|materials = |
||
}} |
}} |
Revision as of 16:03, 30 September 2020
|
About
The Flexus instrument is used to measure the stress introduced onto a wafer after thin-film deposition by measuring local curvature of a wafer. The system uses a scanning laser detector configuration to measure the surface position of a wafer across its diameter. With automatic rotational control, a 3-D map can also be obtained. By comparing before and after measurements of the sample, the local stress of the sample can be calculated from the local curvature. The stage can also be heated up to 500°C to measure thermal mismatch of the thin films with the substrate.
Equipment Specifications
- RT to 500°C operation
- Windows 3.xx control and file storing
- 3-D mapping
- 4" wafers
- Laser/Detector Scanning Configuration