File:PPR220-7 Etch Rates (nm min) vs. Temp(C) Recipe STD O2only 3KW-3min-Temp.png

From UCSB Nanofab Wiki
Revision as of 09:19, 5 June 2023 by Ffoong (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

PPR220-7_Etch_Rates_(nm_min)_vs._Temp(C)_Recipe_STD_O2only_3KW-3min-Temp.png(600 × 371 pixels, file size: 20 KB, MIME type: image/png)

Positive PR etch rates vs temperature

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current09:19, 5 June 2023Thumbnail for version as of 09:19, 5 June 2023600 × 371 (20 KB)Ffoong (talk | contribs)

There are no pages that use this file.