Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeDimensionsUserComment
current18:35, 5 March 2024 (1.38 MB)John d (talk | contribs)added temp and carrier to recipe page
18:33, 5 March 2024 (1.37 MB)John d (talk | contribs)fixed typo in std recipe name
18:22, 5 March 2024 (1.37 MB)John d (talk | contribs)v2, added "std" recipe on top slide.
13:55, 8 October 2021 (1.32 MB)John d (talk | contribs)Oxford Etcher - InP Grating Etch at 20 C - Oxford Cobra 300 2021-08-26 Ning Cao