File:Filmetrics F40-UV - 2018-11-08 - SiO Etch 4m+4m+1m - Fully Removed.png

From UCSB Nanofab Wiki
Revision as of 21:36, 23 May 2019 by John d (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Original file(1,280 × 1,024 pixels, file size: 403 KB, MIME type: image/png)

Filmetrics F40-UV - Example Screenshot of SiO2 etch check, fully removed

File history

Click on a date/time to view the file as it appeared at that time.

Date/TimeThumbnailDimensionsUserComment
current21:36, 23 May 2019Thumbnail for version as of 21:36, 23 May 20191,280 × 1,024 (403 KB)John d (talk | contribs)