File:Au oxidation by O2-N2 ash.jpg

From UCSB Nanofab Wiki
Revision as of 16:17, 9 June 2023 by Ffoong (talk | contribs)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search

Original file(1,388 × 697 pixels, file size: 124 KB, MIME type: image/jpeg)

In high oxidation environment, in this case by O2/N2 mixture recipe, gold surface can oxidize as shown by the XPS data.