Dicing Saw (ADT)

From UCSB Nanofab Wiki
Revision as of 07:58, 16 October 2018 by John d (talk | contribs) (linked to Dicing Recipes)
Jump to navigation Jump to search
Dicing Saw (ADT)
ADT.jpg
Tool Type Packaging
Location Dicing Saw Room
Supervisor Aidan Hopkins
Supervisor Phone (805) 893-2343
Supervisor E-Mail hopkins@ece.ucsb.edu
Description ADT Dicing Saw
Manufacturer Advanced Dicing Technologies Ltd.
Sign up for this tool


About

The ADT 7100 Dicing Saw is optimized for multi-angle dicing of thin, tight tolerance products up to 200 mm x 200 mm. It is currently setup for dicing up to 6” diameter wafers.

Recipes

Be sure to also see the methods for protecting your sample from dicing dust, and mounting/unmounting.