Latest revision as of 03:15, 27 March 2019
- Click on the Programming Workspace
- Go to any recipe
- Click 'Recipe Import'
- Select 'd: [New Volume]' from 'Folder List'
- Open folder 'ADT'. Open Folder 'ADT-7100-8544150816'. Open folder 'db'. Open folder 'exports'
- Find you recipe in the box to the right and double click on it
- Verify group name is correct under 'Recipe Info'
- Click 'OK'
- Click 'Replace'