- Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and ...mperatures, or for materials that have a high risk of contamination in the e-beam evaporators.963 bytes (123 words) - 10:29, 30 August 2022
- |description = Four Pocket Electron Beam Evaporator The Sharon is a cryo-pumped thin film evaporator with a Temescal four hearth 270° bent electron beam evaporation source. Th2 KB (360 words) - 14:44, 3 June 2024
- |description = Load Locked Metal Evaporator Dual Gun ...ration (as low as 20 minutes total time). The system also has two 4-pocket e-beam sources and an Inficon IC/5 deposition controller that allows for co-deposi2 KB (302 words) - 16:30, 22 May 2024
- |description = NRC 3117 Three Source Thermal Evaporator ...rom pumpdown to deposition to system venting is two hours, the same as the e-beam systems.2 KB (382 words) - 17:31, 12 October 2017
- |description = NRC 3117 Three Source Thermal Evaporator ...rom pumpdown to deposition to system venting is two hours, the same as the e-beam systems.3 KB (384 words) - 10:28, 30 August 2022
- *[[Media:Vapor-Pressure-Chart-2.xlsx|Vapor Pressure of Metals (Excel)]] =[[E-Beam 1 (Sharon)]]=8 KB (959 words) - 11:59, 25 October 2022