Difference between revisions of "Resistivity Mapper (CDE RESMAP)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(Updated SOP)
 
(One intermediate revision by the same user not shown)
Line 19: Line 19:
   
 
*[[CDE ResMap Quick-Start instructions]]
 
*[[CDE ResMap Quick-Start instructions]]
  +
*[https://wiki.nanofab.ucsb.edu/w/images/3/37/CDE_ResMap_Operating_Instructions.pdf CDE ResMap Operating Instructions]
 
*System can export CSV files - contact supervisor for instructions.
 
*System can export CSV files - contact supervisor for instructions.

Latest revision as of 15:07, 30 October 2023

Resistivity Mapper (CDE RESMAP)
CDEResmap.jpg
Location Bay ?
Tool Type Inspection, Test and Characterization
Manufacturer Creative Design Engineering
Description CDE Resmap 4 Point Resistivity Mapper

Primary Supervisor Bill Millerski
(805) 893-2655
wmillerski@ucsb.edu

Secondary Supervisor

Tony Bosch


Recipes


About

The CDE Resmap 4 point resistivity mapper is used for measuring resistivity across the wafer for substrates and thin films deposited in the facility. The system can do automated resistivity mapping for pieces to 8 inch wafers.

The resistivity range is 2 mOhm/Square to 5 MOhm/square. Contour plots, 3D plots, histograms, data exporting are supported from the Windows XP based control system.