Difference between revisions of "Tube Furnace (Tystar 8300)"
Jump to navigation
Jump to search
Line 18: | Line 18: | ||
The tubes can hold up to one hundred 8” wafers per tube per cycle. We have boats for various wafer sizes, including pieces. The maximum temperature is 1050°C for the system. Gases used are O<sub>2</sub>, Steam from DI-H<sub>2</sub>O, N<sub>2</sub>. |
The tubes can hold up to one hundred 8” wafers per tube per cycle. We have boats for various wafer sizes, including pieces. The maximum temperature is 1050°C for the system. Gases used are O<sub>2</sub>, Steam from DI-H<sub>2</sub>O, N<sub>2</sub>. |
||
+ | |||
+ | =Useful Information= |
||
+ | [[Media:TystarMechDrawWaferBoat.pdf|Tystar Wafer Boat Drawing - 4" Wafer with 0.5mm Slots]] |
||
=See Also= |
=See Also= |
Revision as of 17:47, 25 September 2013
|
About
The three stack Tystar 8” furnace is used primarily for 3 processes. The processes are dedicated for one tube each:
- SOG curing - Tube 1
- Dry or wet oxidation of silicon - Tubes 2 and 3
- General furnace annealing - Tube 3
The tubes can hold up to one hundred 8” wafers per tube per cycle. We have boats for various wafer sizes, including pieces. The maximum temperature is 1050°C for the system. Gases used are O2, Steam from DI-H2O, N2.
Useful Information
Tystar Wafer Boat Drawing - 4" Wafer with 0.5mm Slots
See Also
- Tystar - Manufacturer of the tool
- Silicon Thermal Oxide Thickness Calculator - Use this on-line calculator to calculate times for silicon oxidation.