= Materials Table =
 
= Materials Table =
  +
For the materials tables, please visit the [[Thermal_Evaporation_Recipes#Materials_Table_(Thermal Evaporator #1)|Thermal Evaporation Recipe Page]].
 
{| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center; font-size: 95%" class="collapsible collapsed wikitable"
 
|-
 
! colspan=6 width=1300 height=35 bgcolor="#D0E7FF" align="center"|<div style="font-size: 150%;">Materials Table</div>
 
|- bgcolor="#D0E7FF"
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Material'''
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Symbol'''
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Density, g/cm3'''
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Z Ratio'''
 
! width="45" bgcolor="#D0E7FF" align="center" | '''Tooling, %'''
 
! width="100" bgcolor="#D0E7FF" align="center" | '''Comments'''
 
|-
 
|Aluminum
 
|Al
 
|2.70
 
|1.08
 
|
 
|
 
|-
 
|Antimony
 
|Sb
 
|6.620
 
|0.768
 
|
 
|
 
|-
 
|Arsenic
 
|As
 
|5.73
 
|0.996
 
|
 
|
 
|-
 
|Beryllium
 
|Be
 
|1.85
 
|0.543
 
|
 
|
 
|-
 
|Boron
 
|B
 
|2.54
 
|0.389
 
|
 
|
 
|-
 
|Cadmium
 
|Cd
 
|8.64
 
|0.682
 
|
 
|
 
|-
 
|Cadmium sulfide
 
|CdS
 
|4.83
 
|1.02
 
|
 
|
 
|-
 
|Cadmium telluride
 
|CdTe
 
|5.85
 
|0.980
 
|
 
|
 
|-
 
|Calcium fluoride
 
|CaF<sub>2</sub>
 
|3.18
 
|0.775
 
|
 
|Used often
 
|-
 
|Carbon (graphite)
 
|C
 
|2.25
 
|3.26
 
|
 
|
 
|-
 
|Chromium
 
|Cr
 
|7.20
 
|0.305
 
|155
 
|Used often
 
|-
 
|Cobalt
 
|Co
 
|8.71
 
|0.343
 
|
 
|
 
|-
 
|Copper
 
|Cu
 
|8.93
 
|0.437
 
|
 
|
 
|-
 
|Gallium
 
|Ga
 
|5.93
 
|0.593
 
|
 
|
 
|-
 
|Gallium Arsenide
 
|GaAs
 
|5.31
 
|1.59
 
|
 
|
 
|-
 
|Germanium
 
|Ge
 
|5.35
 
|0.516
 
|
 
|
 
|-
 
|Gold
 
|Au
 
|19.30
 
|0.381
 
|
 
|Used often
 
|-
 
|Indium
 
|In
 
|7.30
 
|0.841
 
|120
 
|Used often
 
|-
 
|Indium antimonide
 
|InSb
 
|5.76
 
|0.769
 
|
 
|
 
|-
 
|Iridium
 
|Ir
 
|22.4
 
|0.129
 
|
 
|
 
|-
 
|Iron
 
|Fe
 
|7.86
 
|0.349
 
|
 
|
 
|-
 
|Lead
 
|Pb
 
|11.3
 
|1.13
 
|
 
|
 
|-
 
|Lead sulfide
 
|PbS
 
|7.50
 
|0.566
 
|
 
|
 
|-
 
|Lithium fluoride
 
|LiF
 
|2.638
 
|0.778
 
|
 
|
 
|-
 
|Magnesium
 
|Mg
 
|1.74
 
|1.61
 
|
 
|
 
|-
 
|Magnesium oxide
 
|MgO
 
|3.58
 
|0.411
 
|
 
|
 
|-
 
|Magnesium Fluoride
 
|MgF<sub>2</sub>
 
|3.00 ( should be 3.18)
 
|0.427( should be 0.637)
 
|
 
|
 
|-
 
|Manganese
 
|Mn
 
|7.20
 
|0.377
 
|
 
|
 
|-
 
|Manganese(II) Sulfide
 
|MnS
 
|3.99
 
|0.94
 
|
 
|
 
|-
 
|Mercury
 
|Hg
 
|13.46
 
|0.74
 
|
 
|
 
|-
 
|Molybdenum
 
|Mo
 
|10.2
 
|0.257
 
|
 
|
 
|-
 
|Nickel
 
|Ni
 
|8.91
 
|0.331
 
|
 
|Used often
 
|-
 
|Niobium
 
|Nb
 
|8.578
 
|0.492
 
|
 
|
 
|-
 
|Niobium(V) Oxide
 
|Nb<sub>2</sub>O<sub>5</sub>
 
|4.47
 
|*1.00
 
|
 
|*z ratio has not been established
 
|-
 
|Palladium
 
|Pd
 
|12.0
 
|0.357
 
|
 
|
 
|-
 
|Platinum
 
|Pt
 
|21.4
 
|0.245
 
|
 
|
 
|-
 
|Potasium Cloride
 
|KCl
 
|1.98
 
|2.05
 
|
 
|
 
|-
 
|Selenium
 
|Se
 
|4.82
 
|0.864
 
|
 
|
 
|-
 
|Silicon
 
|Si
 
|2.32
 
|0.712
 
|
 
|
 
|-
 
|Silicon(II) Oxide
 
|SiO
 
|2.13
 
|0.87
 
|
 
|
 
|-
 
|Silicon dioxide (fused quarz)
 
|SiO<sub>2</sub>
 
|2.20
 
|1.07
 
|
 
|
 
|-
 
|Silver
 
|Ag
 
|10.5
 
|0.529
 
|
 
|
 
|-
 
|Silver bromide
 
|AgBr
 
|6.47
 
|1.18
 
|
 
|
 
|-
 
|Silver chloride
 
|AgCl
 
|5.56
 
|1.32
 
|
 
|
 
|-
 
|Sodium
 
|Na
 
|0.97
 
|4.8
 
|
 
|
 
|-
 
|Sodium chloride
 
|NaCl
 
|2.17
 
|1.57
 
|
 
|
 
|-
 
|Tantalum
 
|Ta
 
|16.6
 
|0.262
 
|
 
|
 
|-
 
|Tantalum(IV) oxide
 
|Ta<sub>2</sub>O<sub>5</sub>
 
|8.2
 
|0.30
 
|
 
|
 
|-
 
|Tin
 
|Sn
 
|7.30
 
|0.724
 
|
 
|Used often
 
|-
 
|Titanium
 
|Ti
 
|4.50
 
|0.628
 
|
 
|Used often
 
|-
 
|Titanium (IV) Oxide
 
|TiO<sub>2</sub>
 
|4.26
 
|0.40
 
|
 
|
 
|-
 
|Titanium Oxide
 
|TiO
 
|4.90
 
|*1.00
 
|
 
|* z ratio not established
 
|-
 
|Tungsten
 
|W
 
|19.3
 
|0.163
 
|
 
|
 
|-
 
|Tungsten carbide
 
|WC
 
|15.6
 
|0.151
 
|
 
|
 
|-
 
|Zinc
 
|Zn
 
|7.04
 
|0.514
 
|
 
|Used often
 
|-
 
|Zinc Oxide
 
|ZnO
 
|5.61
 
|0.556
 
|
 
|
 
|-
 
|Zinc Sulfide
 
|ZnS
 
|4.09
 
|0.775
 
|
 
|
 
|-
 
|Zirconium
 
|Zr
 
|6.51
 
|0.60
 
|
 
|Should be 6.49
 
|-
 
|Zirconium Oxide
 
|ZrO<sub>2</sub>
 
|5.6
 
|1.001
 
|
 
|
 
|-
 

Revision as of 14:39, 31 March 2014

Thermal Evap 2 (Solder)
Thermal2.jpg
Tool Type Vacuum Deposition
Location Bay 3
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description ?
Manufacturer Custom
Vacuum Deposition Recipes
Sign up for this tool



About

write something...

Detailed Specifications

work on this page...

Documentation

Materials Table

For the materials tables, please visit the Thermal Evaporation Recipe Page.