Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments | ||||||
Aluminum | Al | 2.70 | 1.08 | Antimony | Sb | 2.70 | 0.768 | ||||
Arsenic | As | 5.73 | 0.996 | ||||||||
Beryllium | Be | 1.85 | 0.543 | ||||||||
Boron | B | 2.54 | 0.389 | ||||||||
Cadmium | Cd | 8.64 | 0.682 | ||||||||
Cadmium sulfide | CdS | 4.83 | 1.02 | ||||||||
Cadmium telluride | CdTe | 5.85 | 0.980 | ||||||||
Calcium fluoride | CaF2 | 3.18 | 0.775 | ||||||||
Carbon (graphite) | C | 2.25 | 3.26 | ||||||||
Chromium | Cr | 7.20 | 0.305 | 155 | |||||||
Cobalt | Co | 8.71 | 0.343 | ||||||||
Copper | Cu | 8.93 | 0.437 | ||||||||
Gallium | Ga | 5.93 | 0.593 | ||||||||
Gallium Arsenide | GaAs | 5.31 | 1.59 | ||||||||
Germanium | Ge | 5.35 | 0.516 | ||||||||
Gold | Au | 19.30 | 0.381 | ||||||||
Indium | In | 7.30 | 0.841 | 120 | |||||||
Indium antimonide | InSb | 5.76 | 0.769 | ||||||||
Iridium | Ir | 22.4 | 0.129 | ||||||||
Iron | Fe | 7.86 | 0.349 | ||||||||
Lead | Pb | 11.3 | 1.13 | ||||||||
Lead sulfide | PbS | 7.50 | 0.566 | ||||||||
Lithium fluoride | LiF | 2.64 | 0.774 | ||||||||
Magnesium | Mg | 1.74 | 1.61 | ||||||||
Magnesium oxide | MgO | 3.58 | 0.411 | ||||||||
Magnesium Fluoride | MgF2 | 3.00 | 0.427 | ||||||||
Manganese | Mn | 7.20 | 0.377 | ||||||||
Manganese(II) Sulfide | MnS | 3.99 | 0.94 | ||||||||
Mercury | Hg | 13.46 | 0.74 | ||||||||
Molybdenum | Mo | 10.2 | 0.257 | ||||||||
Nickel | Ni | 8.91 | 0.331 | ||||||||
Niobium | Nb | 8.57 | 0.493 | ||||||||
Niobium(V) Oxide | Nb2O5 | 4.47 | |||||||||
Palladium | Pd | 12.0 | 0.357 | ||||||||
Platinum | Pt | 21.4 | 0.245 | ||||||||
Potasium Cloride | KCl | 1.98 | 2.05 | ||||||||
Selenium | Se | 4.82 | 0.864 | ||||||||
Silicon | Si | 2.32 | 0.712 | ||||||||
Silicon(II) Oxide | SiO | 2.13 | 0.87 | ||||||||
Silicon dioxide (fused quarz) | SiO2 | 2.20 | 1.07 | ||||||||
Silver | Ag | 10.5 | 0.529 | ||||||||
Silver bromide | AgBr | 6.47 | 1.18 | ||||||||
Silver chloride | AgCl | 5.56 | 1.32 | ||||||||
Sodium | Na | 0.97 | 4.8 | ||||||||
Sodium chloride | NaCl | 2.17 | 1.57 | ||||||||
Tantalum | Ta | 16.6 | 0.262 | ||||||||
Tantalum(IV) oxide | Ta2O5 | 8.2 | 0.30 | ||||||||
Tin | Sn | 7.30 | 0.724 | ||||||||
Titanium | Ti | 4.50 | 0.628 | ||||||||
Titanium (IV) Oxide | TiO2 | 4.26 | 0.40 | ||||||||
Titanium Oxide | TiO | 4.90 | N/A | ||||||||
Tangsten | W | 19.3 | 0.163 | ||||||||
Tangsten carbide | WC | 15.6 | 0.151 | ||||||||
Zinc | Zn | 7.04 | 0.514 | ||||||||
Zinc Oxide | Zn | 5.61 | 0.556 | ||||||||
Zinc Sulfide | ZnS | 4.09 | 0.775 | ||||||||
Zirconium | Zr | 6.51 | 0.60 | ||||||||
Zirconium Oxide | ZrO2 | 5.6 |