Sputter 2 (SFI Endeavor)

From UCSB Nanofab Wiki
Revision as of 10:28, 5 September 2018 by John d (talk | contribs) (disclaimer that tool is disabled)
(diff) ← Older revision | Latest revision (diff) | Newer revision → (diff)
Jump to navigation Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
This Tool has been Disabled, and is not available for use any more! These recipes are displayed here for historical/reference purposes only.
Sputter 2 (SFI Endeavor)
Sputter2.jpg
Tool Type Vacuum Deposition
Location Bay 1
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description 3 chamber Cluster Sputter
Manufacturer Endeavor
Vacuum Deposition Recipes
Sign up for this tool


About

This is a three chamber cluster tool for DC and AC reactive sputtering of metals and dielectrics from 8” cylindrical or 2-piece (for AC) targets. The chamber is configured for 4” diameter wafers or equivalently sized plates that can secure smaller piece samples. Samples are loaded into a cassette system capable of holding 20 wafers. The system is computer controlled through a GUI. Heating of the substrate to several hundred degrees Celcius is possible through a heating lamp module. Chamber 1 is set up for AC reactive sputtering of Al, Al2O3, AlN, SiO2, or SiN. Chamber 2 is set up for DC reactive sputtering of Ti, W, TiN, TiO2, and W-based oxides. Chamber 3 is set up for Al or Au metal sputtering and has RF back-sputtering capability on the sample for sample cleaning prior to deposition.

Detailed Specifications

  • Multiple 4” diameter wafer capable system
  • Pieces possible through appropriate carrier design
  • Full programmable control through GUI
  • Heating of substrate to several hundred degrees Celcius
  • Chamber 1: AC sputtering of Si, SiN, SiO2, AlN, Al2O3 films
    • AlN rate ~ 4.5 nm/min.
    • Al2O3 ~ 6 nm/min.
    • SiO2 rate ~ 4.5 nm/min.
  • Chamber 2: DC sputtering of Ti, TiN, TiO2, W, and W-oxides
    • Ti rate ~ 200 nm/min.
  • Chamber 3: DC sputtering of Al or Au. RF back-sputtering with Argon
    • Al Dep rate ~ 300-400 nm/min.


Documentation