Photoluminescence PL Setup (Custom)

From UCSB Nanofab Wiki
Revision as of 14:14, 24 August 2018 by John d (talk | contribs) (header formats)
Jump to navigation Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
Photoluminescence PL Setup (Custom)
Holograph.jpg
Tool Type Inspection, Test and Characterization
Location Bay 6
Supervisor Ning Cao
Supervisor Phone (805) 893-4689
Supervisor E-Mail ningcao@ece.ucsb.edu
Description Custom Built Photoluminescence
Manufacturer NONE



In Progress - incomplete info.

About

The Photoluminescence setup is on the same optical table as the Hologaphic Lithography setup.

Detailed Specifications

Pump Lasers Available

325nm He-Cd - single mode, spatially filtered

405nm Diode Laser

660nm Diode Laser