Difference between revisions of "PECVD Recipes"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 91: Line 91:
 
{| border="1" class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"
 
{| border="1" class="wikitable" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;"
 
|- bgcolor="#D0E7FF"
 
|- bgcolor="#D0E7FF"
!width=350 align=center|50°
+
!width=350 align=center|50° (pinholes)
!width=350 align=center|100°
+
!width=350 align=center|100° (pinholes)
 
!width=350 align=center|250°
 
!width=350 align=center|250°
 
|-align=left
 
|-align=left

Revision as of 15:52, 11 December 2015

Back to Vacuum Deposition Recipes.

PECVD 1 (PlasmaTherm 790)

SiN deposition (PECVD #1)

SiO2 deposition (PECVD #1)

SiOxNy deposition (PECVD #1)

PECVD 2 (Advanced Vacuum)

SiO2 deposition (PECVD #2)

SiN deposition (PECVD #2)

LS SiN deposition (PECVD #2)

Amorphous-Si deposition (PECVD #2)

ICP-PECVD (Unaxis VLR)

SiN deposition (Unaxis VLR)

SiN (2% SiH4)

50° (pinholes) 100° (pinholes) 250°

SiN (2% SiH4 - No-Ar)

50° (pinholes) 100° (pinholes) 250°

SiN (2% SiH4 - No-Ar - Extra N2)

50° 100° 250°

SiN (100% SiH4 )

50° 100° 250°

SiO2 deposition (Unaxis VLR)

SiO2 (2% SiH4)

50° 100° 250°

SiO2 (2% SiH4 - No Ar)

50° 100° 250°

SiO2 (100% SiH4 HDR)

50° 100° 250°

SiO2 (100% SiH4 LDR)

50° 100° 250°

Amorphous Si (100%SiH4 Ar He)

90° 250°