Difference between revisions of "Oven 4 (Thermo-Fisher HeraTherm)"
Jump to navigation
Jump to search
m (John d moved page Oven 4 (Fisher) to Oven 4 (Thermo-Fisher HeraTherm): changed out for new oven) |
|||
(One intermediate revision by one other user not shown) | |||
Line 4: | Line 4: | ||
|super= Tony Bosch |
|super= Tony Bosch |
||
|location=Bay 6 |
|location=Bay 6 |
||
− | |description = |
+ | |description = Programmable Oven |
− | |manufacturer = |
+ | |manufacturer = Thermo Scientific |
+ | |model = HeraTherm |
||
}} |
}} |
||
+ | |||
+ | == About == |
||
+ | This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven. |
||
+ | |||
+ | == Specifications == |
||
+ | * Maximum Temperature = 330 C (no active cooling) |
||
+ | * Gases: N2, manually set with needle valve (not programmable) |
||
+ | * Multi-step programmable temperature ramps |
||
+ | * Programmable atmospheric purge (for cooling) |
||
+ | |||
+ | == Documentation == |
||
+ | * {{todo|User Manual}} |
Revision as of 10:05, 29 October 2019
|
About
This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven.
Specifications
- Maximum Temperature = 330 C (no active cooling)
- Gases: N2, manually set with needle valve (not programmable)
- Multi-step programmable temperature ramps
- Programmable atmospheric purge (for cooling)
Documentation
To Do: User Manual |