+ | =About= |
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH<sub>4,</sub> N<sub>2</sub>, O<sub>2</sub>, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO<sub>2</sub> and Si<sub>3</sub>N<sub>4</sub>, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized. |
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH<sub>4,</sub> N<sub>2</sub>, O<sub>2</sub>, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO<sub>2</sub> and Si<sub>3</sub>N<sub>4</sub>, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized. |
||
+ | ===Cluster Configuration=== |
||
⚫ | |||
+ | A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey. |
||
+ | |||
+ | *'''PM3''': ICP-PECVD Deposition (this page) |
||
+ | *'''PM1''': [[ICP-Etch (Unaxis VLR)|ICP Etch (Unaxis VLR)]] |
||
+ | |||
⚫ | |||
*1000W ICP source, 600W RF Sample Bias Power Supply |
*1000W ICP source, 600W RF Sample Bias Power Supply |
||
Line 23: | Line 29: | ||
=Documentation= |
=Documentation= |
||
+ | |||
− | *[[media:Unaxis_PM3_Web_Operational_Procedure_7-30-13.pdf|Operating Instructions]] |
||
+ | *[//www.nanotech.ucsb.edu/wiki/images/1/1f/Unaxis_PM3_Web_Operational_Procedure_3-27-14.pdf Operating Instructions] |
Revision as of 15:26, 27 November 2019
|
About
This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and 50°C-350°C operation. This chamber has 100% SiH4, N2, O2, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO2 and Si3N4, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be deposited as low as 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized.
Cluster Configuration
A Deposition and Etch chamber are both attached to the same loadlock, allowing etching and deposition without breaking vacuum. Each chamber can be scheduled separately on SignupMonkey.
- PM3: ICP-PECVD Deposition (this page)
- PM1: ICP Etch (Unaxis VLR)
Detailed Specifications
- 1000W ICP source, 600W RF Sample Bias Power Supply
- 50 - 350°C sample temperature
- 100% SiH4, Ar, N2, O2
- Multiple 4” diameter wafer capable system
- Pieces possible by mounting or placing on 4 ” wafer