Holograph.jpg
Tool Type Lithography
Location Bay 6
Supervisor Ning Cao
Supervisor Phone (805) 893-4689
Supervisor E-Mail ningcao@ece.ucsb.edu
Description Custom Built Interference Lithography
Manufacturer Kimmon


About

The interference lithography system at UCSB uses a 15mW, single-mode, 325 nm HeCd laser that is filtered and expanded by pinhole filters to produce the large area exposure beam. The system uses a simple mirror configuration with a fixed 90 degree angle between the mirror and sample. The entire mirror/sample assembly is rotated in 0.1 degree increments to change the grating pitch from ~ 200 nm to ~ 280 nm (35 to 55 degrees) over an ~ 2 cm x 2 cm exposure area. SPR3001 resist spin-coated to ~ 80 nm thickness is used for grating exposure. 2-D gratings can be formed by rotating the sample and doing multiple exposures. Total exposure times are controlled by a manual shutter and are generally several minutes in length.

Detailed Specifications

  • 15 mW single TEM mode HeCd laser
  • ~ 2 cm x 2 cm uniform exposure area
  • ~ several minute exposure times
  • Grating period adjustable from ~200 to ~280 nm with a single stage