Description High Temperature Oven
Manufacturer Blue M Electric


The Blue M oven has a Nitrogen purge and is programmable for up to 8 custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.

Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.