}}The Blue M oven has a Nitrogen purge and is programmable for up to 8 custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.
+
}}The Blue M oven has a Nitrogen purge and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.
   
 
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.
 
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.

Revision as of 19:58, 8 September 2017

High Temp Oven (Blue M)
BlueMOven.jpg
Tool Type Lithography
Location Bay 5
Supervisor Mike Silva
Supervisor Phone (805) 893-3096
Supervisor E-Mail silva@ece.ucsb.edu
Description High Temperature Oven
Manufacturer Blue M Electric


The Blue M oven has a Nitrogen purge and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.

Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.