To Be Added
Detailed Specifications
- Wafer Size: 100mm (150mm possible but not set up)
- PR Coating Properties:
- Uniformity < 1.0%
- < 100 particles on 100mm wafer
- Photoresists/Underlayers Available:
- UV6-0.8
- DS-K101-304
- PMMA
- PMGI SF11
- PMGI SF5
- Solvents Available:
- EBR100
- Developers Available:
- AZ 300 MiF
Process Information
- Recipe Page for S-Cubed Coater: Lithography Recipes > Automated Coat/Develop System Recipes (S-Cubed Flexi)