Difference between revisions of "Wet Etching Recipes"
m (→Compound Semiconductor Etching: update HLink) |
m (update links to master table) |
||
Line 9: | Line 9: | ||
[http://www.sciencedirect.com/science/article/pii/S0927796X00000279 Guide to references on III±V semiconductor chemical etching] |
[http://www.sciencedirect.com/science/article/pii/S0927796X00000279 Guide to references on III±V semiconductor chemical etching] |
||
− | Please add any confirmed etches from this reference to the {{HLink|Wet Etching Recipes|The Master Table of Wet Etching (Include All Materials)}}. |
+ | Please add any confirmed etches from this reference to the {{HLink|Wet Etching Recipes|The Master Table of Wet Etching (Include All Materials)}}. |
==Metal Etching== |
==Metal Etching== |
||
Line 16: | Line 16: | ||
==Silicon etching== |
==Silicon etching== |
||
− | [http://ieeexplore.ieee.org/xpls/abs_all.jsp?arnumber=546406 Etch rates for micromachining processing] |
+ | [http://ieeexplore.ieee.org/xpls/abs_all.jsp?arnumber=546406 Etch rates for micromachining processing] |
− | [http://ieeexplore.ieee.org/xpls/abs_all.jsp?arnumber=1257354 Etch rates for micromachining processing-part II] |
+ | [http://ieeexplore.ieee.org/xpls/abs_all.jsp?arnumber=1257354 Etch rates for micromachining processing-part II] |
+ | |||
+ | Please add any confirmed etches from this reference to the {{HLink|Wet Etching Recipes|The Master Table of Wet Etching (Include All Materials)}}. |
||
==Dielectric etching== |
==Dielectric etching== |
Revision as of 08:32, 18 January 2018
References
Etch rates for Micromachining Processing (IEEE Jnl. MEMS, 1996) - includes tables of etch rates of numerous metals vs. various wet and dry etchants.
Etch rates for micromachining-Part II (IEEE Jnl. MEMS, 2003) - expanded tables containing resists, dielectrics, metals and semiconductors vs. many wet etch chemicals.
Guide to references on III±V semiconductor chemical etching - exhaustive list of wet etchants for etching various semiconductors, including selective etches.
Compound Semiconductor Etching
Guide to references on III±V semiconductor chemical etching
Please add any confirmed etches from this reference to the The Master Table of Wet Etching (Include All Materials).
Metal Etching
- Selective Wet Etch of Cr over Ta using Cr Etchant
- Wet Etch of ITO using Heated, Diluted HCl Solution
Silicon etching
Etch rates for micromachining processing
Etch rates for micromachining processing-part II
Please add any confirmed etches from this reference to the The Master Table of Wet Etching (Include All Materials).
Dielectric etching
Organic removal
Gold Plating
Chemi-Mechanical Polishing (CMP)
Example Wet Etching Table
How to use the Master Table of Wet Etching:
When entering a new etch into the table make a row for every etchant used in the solution such that the information can be sorted by etchant. For example, the InP etch HCl:H3PO4(1:3) and H3PO4:HCl(3:1). Likewise, if etch is known to be selective to multiple materials the etch should have a row for each material. For example HCl:H3PO4(1:3) is selective to both InGaAs and InGaAsP.
This multiple entry method may seem laborious for the person entering a new etch, however the power of sorting by selective materials and chemicals in a table with all materials is great.
Material | Etchant | Rate (nm/min) | Anisotropy | Selective to | Selectivity | Ref. | Notes | Confirmed by | Extra column |
---|---|---|---|---|---|---|---|---|---|
InP | HCl:H3PO4(1:3) | ~1000 | Highly | InGaAs | High | Lamponi (p.102) | Example | Jon Doe | Example |
InP | HCl:H3PO4(1:3) | ~1000 | Highly | InGaAsP | High | Lamponi (p.102) | Example | Jon Doe | Example |
InP | H3PO4:HCl(3:1) | ~1000 | Highly | InGaAs | High | Lamponi (p.102) | Example | Jon Doe | Example |
InP | H3PO4:HCl(3:1) | ~1000 | Highly | InGaAsP | High | Lamponi (p.102) | Example | Jon Doe | Example |
The Master Table of Wet Etching (Include All Materials)
Material | Etchant | Rate (nm/min) | Anisotropy | Selective to | Selectivity | Ref. | Notes | Confirmed by | Extra column |
---|---|---|---|---|---|---|---|---|---|
InP | HCl:H3PO4(1:3) | ~1000 | Highly | InGaAs | High | Lamponi (p.102) | Example | Jon Doe | Example |
InP | HCl:H3PO4(1:3) | ~1000 | Highly | InGaAsP | High | Lamponi (p.102) | Example | Jon Doe | Example |
InP | H3PO4:HCl(3:1) | ~1000 | Highly | InGaAs | High | Lamponi (p.102) | Example | Jon Doe | Example |
InP | H3PO4:HCl(3:1) | ~1000 | Highly | InGaAsP | High | Lamponi (p.102) | Example | Jon Doe | Example |
Al2O3 (ALD Plasma 300C) | 300MIF | ~1.6 | High | Measured in-house | Rate slows with time, Selective to most non-Al Materials | JTB | Example | ||
Al2O3 (ALD Plasma 300C) | 400K | ~2.2 | High | Measured in-house | Rate slows with time, Selective to most non-Al Materials | JTB | Example | ||
Al2O3 (ALD Plasma 300C) | 400K(1:4) | ~1.6 | High | Measured in-house | Rate slows with time, Selective to most non-Al Materials | JTB | Example | ||
Al2O3 (ALD Plasma 300C) | NH4OH:H2O2:H2O (1:2:50) | ~<0.5 | High | Measured in-house | Rate slows with time | JTB | Example | ||
Al2O3 (ALD Plasma 300C) | H2O2:NH4OH:H2O (2:1:50) | ~<0.5 | High | Measured in-house | Rate slows with time | JTB | Example |