There are three standard recipes : STD SiO2, STD Nitride2, and STD LS Nitride2 at 300C. Instructions bellow explain how to run each of the recipes ( seasoning, deposition, cleaning)

STD SiO2

Standard oxide deposition

STD Nitride2

Standard nitride deposition

STD LS Nitride2 at 300C

Standard low stress nitride deposition