Wafer Bonder (SUSS SB6-8E)
Jump to navigation
Jump to search
The printable version is no longer supported and may have rendering errors. Please update your browser bookmarks and please use the default browser print function instead.
|
About
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.
Detailed Specifications
- Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
- Upper and lower heating of samples
- 5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
- Sample size: pieces to 6” wafers, aligned bonding by using the MA/BA-6 aligner - contact supervisor for setup.
- Anodic bonding to 2000 V
- Windows-based computer control
- Wafer bonder currently set up for 4" wafers