Difference between revisions of "Wafer Bonder (SUSS SB6-8E)"
Jump to navigation
Jump to search
(3 intermediate revisions by 2 users not shown) | |||
Line 1: | Line 1: | ||
− | {{ |
+ | {{tool2|{{PAGENAME}} |
|picture=WaferBonder.jpg |
|picture=WaferBonder.jpg |
||
|type = Thermal Processing |
|type = Thermal Processing |
||
− | |super= |
+ | |super= Aidan Hopkins |
+ | |super2= Lee Sawyer |
||
|phone=(805)839-3918x216 |
|phone=(805)839-3918x216 |
||
|location=Bay 7 |
|location=Bay 7 |
||
Line 21: | Line 22: | ||
*Anodic bonding to 2000 V |
*Anodic bonding to 2000 V |
||
*Windows-based computer control |
*Windows-based computer control |
||
+ | *Wafer bonder currently set up for 4" wafers |
Revision as of 10:15, 30 August 2022
|
About
This is Karl-Suss model SB-6 substrate bonder. Wafer bonding of pieces to 6” wafers can be done at pressures from 5e-5 to 3e3 mBar and from 50°C to 550°C. This tool mates with the Karl-Suss MA-6 aligner to allow for aligned bonding. Forces up to 20 kN for a 150 mm wafer size are available. The system supports thermal compression as well as anodic bonding (up to 2000 V). The system is computer controlled with a windows environment allowing for multiple recipe steps and saving of recipes and data. The system is configured for manual loading of wafers.
Detailed Specifications
- Wafer bonding from 50°C to 550°C, +/- 5 degrees accuracy, +/- 3% uniformity
- Upper and lower heating of samples
- 5e-5 to 3e3 Torr environment bonding pressure, with Nitrogen
- Sample size: pieces to 6” wafers, aligned bonding by using MA/BA-6 aligner
- Anodic bonding to 2000 V
- Windows-based computer control
- Wafer bonder currently set up for 4" wafers