Difference between revisions of "Vapor HF Etch"
Jump to navigation
Jump to search
(→About) |
(link to Vapor HF recipes) |
||
Line 15: | Line 15: | ||
=Documentation= |
=Documentation= |
||
− | *[[media:SPTS-Primaxx_uEtch_Presentation-a.pdf|System Manual]] |
+ | *[[media:SPTS-Primaxx_uEtch_Presentation-a.pdf|System Manual Part A]] |
− | *[[media:SPTS-Primaxx_uEtch_Presentation-b.pdf|System Manual]] |
+ | *[[media:SPTS-Primaxx_uEtch_Presentation-b.pdf|System Manual Part B]] |
+ | |||
− | *[[media:25-Dry_Etch_of_Unaxis_ICP-grown_SiO2_using_Vapor_HF_tool-a.pdf|Si Etching Profile & Results]] |
||
+ | =Recipes= |
||
− | *[[media:26-Dry_Etch_of_Unaxis_ICP-grown_SiO2_using_Vapor_HF_tool-b.pdf|Si Etching Profile & Results]] |
||
+ | See the [https://www.nanotech.ucsb.edu/wiki/index.php/Other_Dry_Etching_Recipes#Vapor_HF_Etch_.28uETCH.29 Vapor HF Recipes] page |
Revision as of 10:03, 30 April 2018
|
About
The applications of this tool are mainly in MEMS-device fabrication areas (releasing a MEMS structure by etching a sacrificial SiO2 layer below) with the use of Al2O3, Al or some other metal as an etch mask at 45oC. The tool uses vapor HF (VHF), EtOH (Ethanol vapor is an Alcohol-based one, ionizing the HF and activating etching, influencing within wafer etch uniformity, and being most compatible with VHF), and N2 gases and can process small sample(s) (on a 8" Si carrier wafer) up to an 8" wafer. There are 5 standard etch recipes installed in the tool with the SiO2 undercut-etch-rate from low to high. The SiO2 undercut-etch-rate is from ~10nm/min to ~350nm/min.
Documentation
Recipes
See the Vapor HF Recipes page