Difference between revisions of "Vacuum Deposition Recipes"
Jump to navigation
Jump to search
Line 1: | Line 1: | ||
− | {| border="1 |
+ | {| border="1" style="border: 1px solid #D0E7FF; background-color:#ffffff; text-align:center;" class="wikitable" |
|- bgcolor="#D0E7FF" |
|- bgcolor="#D0E7FF" |
||
! width="1675" height="45" colspan="18" | <div style="font-size: 150%;">Vacuum Deposition Recipes</div> |
! width="1675" height="45" colspan="18" | <div style="font-size: 150%;">Vacuum Deposition Recipes</div> |
||
Line 484: | Line 484: | ||
| {{rl|PECVD Recipes|SiN deposition (Unaxis VLR)}} |
| {{rl|PECVD Recipes|SiN deposition (Unaxis VLR)}} |
||
| <br> |
| <br> |
||
− | | {{rl |
+ | | {{rl|Ion Beam Deposition Recipes|SiN deposition (IBD)}} |
| <br> |
| <br> |
||
|- |
|- |