Difference between revisions of "Vacuum Deposition Recipes"
Jump to navigation
Jump to search
m (link to sputter 5 section) |
m (fixed AJA3 Cr link) |
||
Line 209: | Line 209: | ||
| <br> |
| <br> |
||
| <br> |
| <br> |
||
+ | | [https://www.nanotech.ucsb.edu/wiki/index.php/Sputtering_Recipes#Sputter_3_.28AJA_ATC_2000-F.29 R] |
||
− | | [[Sputtering Recipes|R]] |
||
| <br> |
| <br> |
||
| <br> |
| <br> |
Revision as of 18:15, 29 November 2018
- R = Recipe is available. Clicking this link will take you to the recipe.
- A = Material is available for use, but no recipes are provided.