Difference between revisions of "Tube Furnace (Tystar 8300)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 4: Line 4:
 
|super= Tony Bosch
 
|super= Tony Bosch
 
|phone=(805)839-3918x217
 
|phone=(805)839-3918x217
|location=Bay 3
+
|location=Bay 4
 
|email=bosch@ece.ucsb.edu
 
|email=bosch@ece.ucsb.edu
 
|description = Tystar 8" 3-Tube Oxidation/Annealing System
 
|description = Tystar 8" 3-Tube Oxidation/Annealing System

Revision as of 10:15, 28 June 2012

Tube Furnace (Tystar 8300)
Tystar.jpg
Tool Type Thermal Processing
Location Bay 4
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description Tystar 8" 3-Tube Oxidation/Annealing System
Manufacturer Tystar Corporation


About

The three stack Tystar 8” furnace is used primarily for 3 processes. The processes are dedicated for one tube each:

  1. Dry or wet oxidation of silicon - Tubes 2 and 3
  2. SOG curing - Tube 1
  3. General furnace annealing - Tube 3

The tubes can hold up to one hundred 8” wafers per tube per cycle. We have boats for various wafer sizes, including pieces. The maximum temperature is 1050°C for the system. Gases used are O2, Steam from DI-H2O, N2.