Thermal Evap 2 (Solder)
|
About
Materials Table
Materials Table
| |||||
---|---|---|---|---|---|
Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
Aluminum | Al | 2.70 | 1.08 | ||
Antimony | Sb | 2.70 | 0.768 | ||
Arsenic | As | 5.73 | 0.996 | ||
Beryllium | Be | 1.85 | 0.543 | ||
Boron | B | 2.54 | 0.389 | ||
Cadmium | Cd | 8.64 | 0.682 | ||
Cadmium sulfide | CdS | 4.83 | 1.02 | ||
Cadmium telluride | CdTe | 5.85 | 0.980 |