Thermal Evap 2 (Solder)
|
About
Materials Table
Materials Table
| |||||
---|---|---|---|---|---|
Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
Aluminum | Al | 2.70 | 1.08 | Tooling factor, % | Comment |
|
Materials Table
| |||||
---|---|---|---|---|---|
Material | Symbol | Density, g/cm3 | Z Ratio | Tooling, % | Comments |
Aluminum | Al | 2.70 | 1.08 | Tooling factor, % | Comment |