Difference between revisions of "Thermal Evap 2 (Solder)"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Line 86: Line 86:
 
|0.775
 
|0.775
 
|
 
|
|
+
|Used often
 
|-
 
|-
 
|Carbon (graphite)
 
|Carbon (graphite)
Line 100: Line 100:
 
|0.305
 
|0.305
 
|155
 
|155
|
+
|Used often
 
|-
 
|-
 
|Cobalt
 
|Cobalt
Line 149: Line 149:
 
|0.841
 
|0.841
 
|120
 
|120
|
+
|USed often
 
|-
 
|-
 
|Indium antimonide
 
|Indium antimonide
Line 247: Line 247:
 
|0.331
 
|0.331
 
|
 
|
|
+
|Used often
 
|-
 
|-
 
|Niobium
 
|Niobium
Line 366: Line 366:
 
|0.724
 
|0.724
 
|
 
|
|
+
|USed often
 
|-
 
|-
 
|Titanium
 
|Titanium
Line 373: Line 373:
 
|0.628
 
|0.628
 
|
 
|
|
+
|Used often
 
|-
 
|-
 
|Titanium (IV) Oxide
 
|Titanium (IV) Oxide
Line 408: Line 408:
 
|0.514
 
|0.514
 
|
 
|
|
+
|Used often
 
|-
 
|-
 
|Zinc Oxide
 
|Zinc Oxide

Revision as of 10:23, 29 August 2012

Thermal Evap 2 (Solder)
Thermal2.jpg
Tool Type Vacuum Deposition
Location Bay 3
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description ?
Manufacturer Custom
Vacuum Deposition Recipes
Sign up for this tool



About

Materials Table