Line 82: Line 82:
 
|-
 
|-
 
|Calcium fluoride
 
|Calcium fluoride
|CaF2
+
|CaF<sub>2</sub>
 
|3.18
 
|3.18
 
|0.775
 
|0.775

Revision as of 08:03, 29 August 2012

Thermal Evap 2 (Solder)
Thermal2.jpg
Tool Type Vacuum Deposition
Location Bay 3
Supervisor Brian Lingg
Supervisor Phone (805) 893-8145
Supervisor E-Mail lingg_b@ucsb.edu
Description ?
Manufacturer Custom
Vacuum Deposition Recipes
Sign up for this tool



About

Materials Table