Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin.  
+
Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. See the Recipes section below for other materials used.  
  
 
Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.
 
Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.
Line 24: Line 24:
 
== Recipes ==
 
== Recipes ==
 
* [[Thermal Evaporation Recipes#Thermal Evaporator 2|Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2]]  
 
* [[Thermal Evaporation Recipes#Thermal Evaporator 2|Recipes > Thermal Evaporation Recipes > Thermal Evaporator 2]]  
** ''Visit this page for the materials tables and evaporation parameters.''
+
** ''Visit this page for the materials table and evaporation parameters for all materials available.''

Latest revision as of 09:27, 19 May 2020

Thermal Evap 2 (Solder)
Thermal2.jpg
Tool Type Vacuum Deposition
Location Bay 3
Supervisor Don Freeborn
Supervisor Phone (805) 893-7975
Supervisor E-Mail dfreeborn@ece.ucsb.edu
Description ?
Manufacturer Custom
Vacuum Deposition Recipes
Sign up for this tool



About

Thermal evaporator #2 is the designated "Solder" evaporator. The tool is used primarily for solder materials including Gold, Indium and Tin. See the Recipes section below for other materials used.

Use this tool for materials with low melting temperatures, or for materials that have a high risk of contamination in the e-beam evaporators.

Detailed Specifications

Wafers up to 12" can be mounted.

Documentation

Recipes