Difference between revisions of "Test Data of etching SiO2 with CHF3/CF4/O2 (using this recipe only for Fluorine etch of the underneath layer)"
Jump to navigation
Jump to search
(add data) |
(add a pic) |
||
Line 36: | Line 36: | ||
|0.69 |
|0.69 |
||
|78.1 |
|78.1 |
||
+ | |[https://www.nanotech.ucsb.edu/wiki/images/0/04/I2190605.pdf] |
||
− | | |
||
|} |
|} |