Difference between revisions of "Test Data of etching SiO2 with CHF3/CF4/O2"
Jump to navigation
Jump to search
(add data file) |
(add a table) |
||
Line 1: | Line 1: | ||
+ | {| class="wikitable" |
||
+ | | colspan="5" |ICP#2: 0.5Pa, 50/500W, CHF3/CF4/O2=35/5/10sccm, time=210 sec |
||
+ | |- |
||
+ | |Date |
||
+ | |Sample# |
||
+ | |Etch Rate (nm/min) |
||
+ | |Etch Selectivity (SiO2/PR) |
||
+ | |Averaged Sidewall Angle (<sup>o</sup>) |
||
+ | |- |
||
+ | |10/5/2018 |
||
+ | |SiO2#01 |
||
+ | |95.2 |
||
+ | |0.74 |
||
+ | |77.9 |
||
+ | |} |
||
[[:File:SiO2 Etch using ICP2 with O2.pdf]] |
[[:File:SiO2 Etch using ICP2 with O2.pdf]] |
Latest revision as of 16:17, 8 October 2018
ICP#2: 0.5Pa, 50/500W, CHF3/CF4/O2=35/5/10sccm, time=210 sec | ||||
Date | Sample# | Etch Rate (nm/min) | Etch Selectivity (SiO2/PR) | Averaged Sidewall Angle (o) |
10/5/2018 | SiO2#01 | 95.2 | 0.74 | 77.9 |