Florine ICP: 3.8mT, 50/800W, CHF3/CF4=10/30sccm, and Time=90 sec
Date Sample# Etch Rate (nm/min) Etch Selectivity (SiO2/PR) Averaged Sidewall Angle (o) SEM Images
1/28/2021 FE2102 309 0.99 [1]