(Created page with "{| class="wikitable" | colspan="6" |Fluorine ICP: 3.8mT, 50/800W, CHF3/CF4=10/30sccm, time=90 sec |- |Date |Sample# |Etch Rate (nm/min) |Etch Selectivity (SiO2/PR) |Average...")
 
 
Line 14: Line 14:
 
|0.99
 
|0.99
 
|
 
|
|
+
|[https://wiki.nanotech.ucsb.edu/w/images/0/0b/FE210206.pdf]
 
|}
 
|}

Latest revision as of 16:16, 4 February 2021

Fluorine ICP: 3.8mT, 50/800W, CHF3/CF4=10/30sccm, time=90 sec
Date Sample# Etch Rate (nm/min) Etch Selectivity (SiO2/PR) Averaged Sidewall Angle (o) SEM Images
1/28/2021 FE2102 309 0.99 [1]