Difference between revisions of "Template:Recipe"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(format noinclude text)
m
Line 3: Line 3:
 
-->
 
-->
 
<noinclude>''The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.''</noinclude>
 
<noinclude>''The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.''</noinclude>
  +
==Recipe==
 
   
 
<includeonly>[[category:Recipes]]</includeonly>
 
<includeonly>[[category:Recipes]]</includeonly>
 
==Recipe==
 
;Recipe Name
 
;Recipe Name
 
: SiOVert_MadeUp
 
: SiOVert_MadeUp

Revision as of 14:56, 3 August 2017

The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.


Recipe

Recipe Name
SiOVert_MadeUp
Tool
Panasonic ICP #2
Description
This recipe is made up, and deposits glass with lots of holes in it.
Recipe Parameters
Ar = 20 sccm
O2 = 10 sccm
Pressure = 50 mT
RF = 200 W
Temperature = 200°C
Dep Rate
200 nm/min or 12,000 nm/sec
Notes
Make sure sample is inside out before loading into tool.
This recipe usually doesn't work.
Film will etch in HF

Characterization

Al-thickness-variation-with-rate.jpg