Difference between revisions of "Template:Recipe"
Jump to navigation
Jump to search
(comment help) |
m |
||
(3 intermediate revisions by the same user not shown) | |||
Line 2: | Line 2: | ||
Use the Definition List syntax, where ; denotes a title and : denotes a new line for the list under that item. |
Use the Definition List syntax, where ; denotes a title and : denotes a new line for the list under that item. |
||
--> |
--> |
||
− | <noinclude>The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.</noinclude> |
+ | <noinclude>''The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.''</noinclude> |
⚫ | |||
− | |||
<includeonly>[[category:Recipes]]</includeonly> |
<includeonly>[[category:Recipes]]</includeonly> |
||
⚫ | |||
;Recipe Name |
;Recipe Name |
||
: SiOVert_MadeUp |
: SiOVert_MadeUp |
Latest revision as of 14:56, 3 August 2017
The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.
Recipe
- Recipe Name
- SiOVert_MadeUp
- Tool
- Panasonic ICP #2
- Description
- This recipe is made up, and deposits glass with lots of holes in it.
- Recipe Parameters
- Ar = 20 sccm
- O2 = 10 sccm
- Pressure = 50 mT
- RF = 200 W
- Temperature = 200°C
- Dep Rate
- 200 nm/min or 12,000 nm/sec
- Notes
- Make sure sample is inside out before loading into tool.
- This recipe usually doesn't work.
- Film will etch in HF