Difference between revisions of "Template:Recipe"
Jump to navigation
Jump to search
(1st attempt, using definition list) |
m |
||
(5 intermediate revisions by the same user not shown) | |||
Line 1: | Line 1: | ||
+ | <!-- Please replace the recipe name and other info with your own. |
||
+ | Use the Definition List syntax, where ; denotes a title and : denotes a new line for the list under that item. |
||
+ | --> |
||
+ | <noinclude>''The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.''</noinclude> |
||
<includeonly>[[category:Recipes]]</includeonly> |
<includeonly>[[category:Recipes]]</includeonly> |
||
+ | ==Recipe== |
||
;Recipe Name |
;Recipe Name |
||
: SiOVert_MadeUp |
: SiOVert_MadeUp |
||
+ | |||
+ | ;Tool |
||
+ | : Panasonic ICP #2 |
||
;Description |
;Description |
||
Line 20: | Line 28: | ||
: This recipe usually doesn't work. |
: This recipe usually doesn't work. |
||
: Film will etch in HF |
: Film will etch in HF |
||
+ | |||
+ | ----- |
||
+ | |||
+ | ==Characterization== |
||
+ | [[File:Al-thickness-variation-with-rate.jpg]] |
Latest revision as of 14:56, 3 August 2017
The recipe shown here is just a placeholder - please replace this info with your own. This text won't show up in the final page.
Recipe
- Recipe Name
- SiOVert_MadeUp
- Tool
- Panasonic ICP #2
- Description
- This recipe is made up, and deposits glass with lots of holes in it.
- Recipe Parameters
- Ar = 20 sccm
- O2 = 10 sccm
- Pressure = 50 mT
- RF = 200 W
- Temperature = 200°C
- Dep Rate
- 200 nm/min or 12,000 nm/sec
- Notes
- Make sure sample is inside out before loading into tool.
- This recipe usually doesn't work.
- Film will etch in HF